Synthesis and Characterization of Nano-Multilayer Graphene Grown by Ambient Pressure of Chemical Vapor Deposition from Naphthalene/Methanol

Document Type : Research Paper

Authors

1 Chemistry Department, College of Science Diyala University, Iraq

2 Chemistry Department , College of Education for Pure Science -Ibn AL-Haytham, University of Baghdad, Iraq

3 Forensic Evidence Department, College of Science, Al-Karkh University of Science, Iraq

4 Pharmaceutics Department, College of Pharmacy, University of Babylon, Hilla, Iraq

10.22052/JNS.2023.03.023

Abstract

Multilayer graphene was synthesized by chemical vapor deposition from mixture of naphthalene/ methanol with ratios (1.5 g: 100 m L) respectively at ambient pressure and nitrogen as carrier gas with two different flow at 700 °C. The active sites for growth was Ferrocene with thickness reach to125 μm. The product was characterized by Raman spectroscopy, scanning electron microscopy, and Energy Dispersive X-Ray Analysis. The analysis shows that high flow of carrier gas (250 cm3/min) was succeeded to produce graphene multilayers while the ether (100 cm3/min) witnessed many tubular structure in addition to graphene layers.

Keywords


INTRODUCTION

Despite of appearance carbon nanotubes CNTs and fullerene after 1990s but graphite and graphene did not lost their shining so, they remained occupied huge attention on the world in many fields. Many literatures were [1] reported different techniques for synthesized graphene such physical and chemical exfoliation , oxidation of graphite by different oxidation reagents, physical vapor deposition, laser irradiation[2] and chemical vapor deposition (CVD) [3] . All the methods can produces few–sheets of graphene and graphite when choosing the specific condition for preparation. Mostly the CVDs represent the best method for synthesized quantitative and qualitative planer and tubular of carbon which represent by carbon nanotubes CNTs and graphene respectively [4]. Ryuichi and Masataka were developed CVDs with plasma to synthesis [5] thin film of graphene at 1300 °C.  Duygu et al. [6] was used a combined method of high-energy ball milling and ~0.57 Torr of pressure CVDs to synthesized Graphite-encapsulated Fe nanoparticles   from CH4/H2 at 1050°C. 

Aparna et al. [7]were prepared Few layer graphene by combining ball milling with exfoliants from low-cost graphite, in an aqueous medium containing a strong exfoliant (1-pyrenecarboxylic acid) and Methanol. Zoran and Silvio [8] design a very low-cost CVDs reactor for synthesized high quality single and multi-layer graphene at less than 1000°C from methanol with foil made of transition metals as catalyst for growth. Zhen et al. [9] succeeded to synthesized centimeter-scale single- to few-layer graphene films by CVD on Ni foils from mixture Methane/H2/Ar at 900°C. Cortes et al. [10] used acetylene as carbon source to synthesized Few-layer graphene by CVDs on a CuO deposited by sputtering over SiO2/Si substrates without post processing to transfer the CuO onto a dielectric substrate or the use of ultra-high vacuum during synthesis.

May et al. [11] used bi-metallic Co-Ni oxide/Al2O3 substrate in CVDs method to synthesized   multilayer graphene   at a temperature range of 700-900 °C. Allaedini et al.[12] prepared few-layered graphene using (CVD) method with Ni–Ce–Fe as tri-metallic catalyst by using Carbon dioxide as the carbon source at 800°C. Hyosub et al. [13] synthesized Graphene with 2-3 layers was prepared on 100 μm-thick Fe foil as catalyst at low temperature by CVDs from acetylene as a hydrocarbon source.  The studies shows that increase flow rate  of acetylene from 5 cm3 to 25-50 cm3  and increase the exposure time from 5 min to 15-30 min , causing increase the thickness of graphene layer. 

In this work multi-layers of graphene was synthesized from Naphthalene/methanol mixture as source of carbon in CVDs method at 700 °C and Ferrocene as catalyst on SiO2 support. 

 

MATERIALS AND METHODS

Materials

Naphthalene from Sigma-Aldrich with 99% in purities, solvent Methanol (99.85%) from Hyman, England and Nitrogen gas N2 as carrier gas with purities 99.999% was purchase from Emirates industrial gases. Ferrocene Fe (C5H5)2 as catalyst sources was purchased from Sigma and Nitric acid   (70%) from Fisher was used for purification.

 

Synthesis process

Chemical vapor deposition was applied by mono-stage tube furnace (XIN YOO electronic components co. Ltd.) from Chania equipped with a quartz tube, 1.60 cm in length and 5 cm in diameter. The sources of carbon was solution of Naphthalene/Methanol (1.5g: 100 mL) which evaporated at 90°C. Fig. 1, shows the skim for CVDs system where two types of the graphene multi sheets was synthesized by CVD at ambient pressure. A ferrocene with ≈125 μm thick was used as catalyst over (3×7.2 cm2) SiO2 support. Before the precipitation, the catalyst/substrate was baked on tube furnace at 700 °C in an atmosphere of N2 (250 cm3/min) for 10 min to precipitation Fe on the support. The synthesis was done for 30 min. at 700°C, and 250 cm3/min consumption rates of realized N2 for the first sample which a sign (G-250). The second samples (G-100) was synthesis at the same conditions with reduce the flow rate of N2 gas to 100 cm3/min. After deposition the furnace was switched off and allowed to cool at room temperature under a continuous N2 flow, then the product was purified by reflex with 1 M of HCl for 6 hours at 80 °C. 

 

RESULTS AND DISCUSSION

The Raman spectroscopy was done by Sentara Infinity Bruker 1, for the range from 100 cm-1 – 3500 cm-1.  Scanning electron microscopy SEM, JEOL – JSM-6700F Japan with EDX system were used to shows the nature of surface and morphology with elements analysis for the synthesized materials.

The Graphene or graphite peak created from the first-order scattering process of the double vibration’s degenerate phonon of center Brillouin zone which is due to sp2 bonded carbon, while, the disordered structure of the graphene edges sheets in graphene was represent by D band [14]. Mostly Measurement of 𝐼G/𝐼D ratio is a well-known method for characterization the nature structure and disorder [15] for tubular graphene or graphite. The high intensity for 2D for graphite and graphene make it suitable to identify the nature of planer graphene and graphite by measurement the ratios of 𝐼2D/𝐼G [16]. However the identification parameters between tubular structure and planer structure of sp2 carbon was the intensity ratios of 2D. The evaluation of the synthesized graphene structure G-250 and G-100 required Raman spectroscopy to probe structural and physical properties of graphitic materials, such disorder, defects, charges, and strain [17]. The Raman spectroscopy shows the D, G, and 2D bands for G-250 at 1360 cm−1, 1584 cm−1, and 2740 cm−1 respectively, the G-100 were 1348cm-1, 1548 cm-1 while 2D band was very week (Fig. 2). Raise 2D for first sample G-250 refer to forming graphene with multi-sheets while reduce or weakness 2D for the second sample indicate to low ratios of graphene sheets [18].  

May be the reason behind week intensity for 2D peaks due to interference with D+G peak due to forming tubular structure of graphene with the product as shown in SEMs images. 

Fig. 3, and 4 include the SEM images for the two samples, the first, shows 3a and 4a bulk material for synthesized products. Fig. 3b, c and d shows different scale for G-250 which shows many planar fragments without any filaments structures. Fig. 4b, c and d shows many scales for the second sample include the many sheets of graphene with many agglomerate for filament of CNTs which mostly refer to MWCNTs. 

The EDXs analysis of the prepared two samples are presented in Fig. 5, Which confirms that carbon is the dominant atomic composition when forming 68.36% and 45.06% for G-250 and G-100 respectively. The two samples contained oxygen with 5.34% and 8.13% respectively, in addition to present Fe, Si, Al, Au, Ca and Mo, which are the elements of the catalyst and support of catalyst. Carbon in the first sample has the highest weight percent compare the ether, and that may be refer to adequate ratios of  the flow rate for carrier gas  has played an active role in the CVDs system to  producing graphene.

The phase diagrams of Fe necessary to predict the mechanism at the temperature of reaction in CVDs. The overall outcome of graphene synthesis, depend on Fe relatively high carbon solubility and that explained by phase diagram. Fig. 6, shows the phase diagram [19] it is notable that the solubility of carbon can reach a maximum of Fe is estimated to have the carbon solubility of >25 %. The temperature of precipitation in this work, was 700 °C and the carbon solubility decreases to reach less than 1% causing spontaneous carbon precipitation to gives graphene during the cooling stage, [20].

Chemical vapor deposition for the formation of graphene on Fe sites include a two-step [22]. The first step is the dilution or incorporation of carbon into the metal (dissolution), then followed by segregation when the graphene was formed after rapid cooling. 

The suppose mechanism for graphene formation by the precipitation free radical/segregation process on the support with Fe catalyst was listed in equation 1 to equation 6. The mechanism have been agreement with Blakely’s group [23] , when supposed the segregation compositional involves heterogeneity in thermal equilibrium under conditions that correspond to one phase field in the phase diagram [21] whereas precipitation indicates the inhomogeneity due to the equilibrium phase separation [24]. The process required chemisorbs by the empty d-shell (1) for the hydrocarbon on the metal surface which followed by dissociates (2) through dehydrogenation, and the dissolute carbon (3) atoms will diffuse into the bulk metal. The last steps enhance the diffuse excess carbon to the surface (4), before the last step when (5) the segregation forming graphene which continues to produce graphite (6).

          

The chemisorption was active due to the empty d-shell/ an electron acceptor between Fe catalyst and free radicals respectively [25]. The segregation is responsible to make active site for growth by nucleation process which continues until the concentration of free radical in the bulk metal has reduce to reach equilibrium, [25] with nucleation. 

The reason behind including G-250 graphene sheets only while G-100 shows a set of tubular structures in addition to graphene with high ratios of impurities can summarized to three reasons: i-From the phase diagram shows that the ability of Fe to saturation with carbon is low thus, the low flow velocity 100 cm3/min enabled carbon free radicals to react with Fe. The high flow at 250 cm3/min make the precipitation to accrue vastly without reactant with Fe. ii-the suppose mechanism by [26], mentions that graphene can be formed before reaching to Fe/SiO2 and that kinetically favorite at high flow and that reduce the probabilities to react Fe with graphene. iii- Thermodynamically graphene more stable then CNTs[27] thus, high flow at 250 cm3/min make the probabilities for collision free radicals and forming graphene was easier than low rate which prefer to form CNTs. 

 

CONCLUSION

Graphene multi layers were synthesized at ambient pressure with two different flows of carrier’s gas which shows critical parameters and important requirement to decided planer or tubular structure of carbon material. Thus, the functional analysis with spectroscopic images technique showed that catalyst at the conditions of preparation carbon sheets at 700∘C unnecessary requirement for the synthesis of graphene. The results showed that flow of carrier gases can play important parameter for built carbon sheets or tubular structure when provided the ideal condition for diffusion with rearrange the donor with accepter electrons to forming uniform sheets or multi-form structures.

 

CONFLICT OF INTEREST

The authors declare that there is no conflict of interests regarding the publication of this manuscript.

1. Bhuyan MSA, Uddin MN, Islam MM, Bipasha FA, Hossain SS. Synthesis of graphene. International Nano Letters. 2016;6(2):65-83.
2. Wu Y, Wang S, Komvopoulos K. A review of graphene synthesis by indirect and direct deposition methods. Journal of Materials Research. 2020;35(1):76-89.
3. Muñoz R, Gómez-Aleixandre C. Review of CVD Synthesis of Graphene. Chemical Vapor Deposition. 2013;19(10-11-12):297-322.
4. Dinadayalane TC, Leszczynski J. Fundamental Structural, Electronic, and Chemical Properties of Carbon Nanostructures: Graphene, Fullerenes, Carbon Nanotubes, and Their Derivatives. Handbook of Computational Chemistry: Springer International Publishing; 2017. p. 1175-1258.
5. Kato R, Hasegawa M. Fast synthesis of thin graphite film with high-performance thermal and electrical properties grown by plasma CVD using polycrystalline nickel foil at low temperature. Carbon. 2019;141:768-773.
6. Ağaoğulları D, Madsen SJ, Ögüt B, Koh AL, Sinclair R. Synthesis and characterization of graphite-encapsulated iron nanoparticles from ball milling-assisted low-pressure chemical vapor deposition. Carbon. 2017;124:170-179.
7. Aparna R, Sivakumar N, Balakrishnan A, Sreekumar Nair A, Nair SV, Subramanian KRV. An effective route to produce few-layer graphene using combinatorial ball milling and strong aqueous exfoliants. Journal of Renewable and Sustainable Energy. 2013;5(3).
8. Ereš Z, Hrabar S. Low-cost synthesis of high-quality graphene in do-it-yourself CVD reactor. Automatika. 2018;59(3-4):254-260.
9. Juang Z-Y, Wu C-Y, Lu A-Y, Su C-Y, Leou K-C, Chen F-R, Tsai C-H. Graphene synthesis by chemical vapor deposition and transfer by a roll-to-roll process. Carbon. 2010;48(11):3169-3174.
10. CortÉS A, CeledÓN C, Zarate R. CVD synthesis of graphene from acetylene catalyzed by a reduced CuO thin film deposited on SiO2 substrates. Journal of the Chilean Chemical Society. 2015;60(2):2911-2913.
11. Ali M, Rashid SA, Hamidon MN, Md Yasin F. Facile Synthesis and Characterization of Multi-Layer Graphene Growth on Co-Ni Oxide/Al2O3 Substrate Using Chemical Vapour Deposition. Bulletin of Chemical Reaction Engineering & Catalysis. 2018;13(2):341-354.
12. Allaedini G, Tasirin SM, Aminayi P. Synthesis of graphene through direct decomposition of CO2 with the aid of Ni–Ce–Fe trimetallic catalyst. Bulletin of Materials Science. 2016;39(1):235-240.
13. An H, Lee W-J, Jung J. Graphene synthesis on Fe foil using thermal CVD. Current Applied Physics. 2011;11(4):S81-S85.
14. Reichardt S, Wirtz L. Ab initio calculation of the peak intensity of graphene: Laser-energy and Fermi-energy dependence and importance of quantum interference effects. Physical Review B. 2017;95(19).
15. Cançado LG, Jorio A, Ferreira EHM, Stavale F, Achete CA, Capaz RB, et al. Quantifying Defects in Graphene via Raman Spectroscopy at Different Excitation Energies. Nano Letters. 2011;11(8):3190-3196.
16. Malard LM, Pimenta MA, Dresselhaus G, Dresselhaus MS. Raman spectroscopy in graphene. Physics Reports. 2009;473(5-6):51-87.
17. Moreno-Bárcenas A, Perez-Robles JF, Vorobiev YV, Ornelas-Soto N, Mexicano A, García AG. Graphene Synthesis Using a CVD Reactor and a Discontinuous Feed of Gas Precursor at Atmospheric Pressure. Journal of Nanomaterials. 2018;2018:1-11.
18. Han J, Lee J-Y, Yeo J-S. Large-area layer-by-layer controlled and fully bernal stacked synthesis of graphene. Carbon. 2016;105:205-213.
19. American Society for Metals Changes Name to ASM International. Bulletin of Alloy Phase Diagrams. 1987;8(1):2-2.
20. An H, Lee WG, Jung J. Graphene Growth on Sidewall of Catalyst by CVD and Its Application to Graphene Transistors.  Extended Abstracts of the 2011 International Conference on Solid State Devices and Materials; 2011/09/30: The Japan Society of Applied Physics; 2011.
21. Atkins P, Paula Jd, Smith D. Solubility equilibria. Elements of Physical Chemistry: Oxford University Press; 2016.
22. Seah C-M, Chai S-P, Mohamed AR. Mechanisms of graphene growth by chemical vapour deposition on transition metals. Carbon. 2014;70:1-21.
23. Shelton JC, Patil HR, Blakely JM. Equilibrium segregation of carbon to a nickel (111) surface: A surface phase transition. Surface Science. 1974;43(2):493-520.
24. Li X, Cai W, Colombo L, Ruoff RS. Evolution of Graphene Growth on Ni and Cu by Carbon Isotope Labeling. Nano Letters. 2009;9(12):4268-4272.
25. Loginova E, Bartelt NC, Feibelman PJ, McCarty KF. Factors influencing graphene growth on metal surfaces. New Journal of Physics. 2009;11(6):063046.
26. Nessim GD. Properties, synthesis, and growth mechanisms of carbon nanotubes with special focus on thermal chemical vapor deposition. Nanoscale. 2010;2(8):1306.
27. Mostofizadeh A, Li Y, Song B, Huang Y. Synthesis, Properties, and Applications of Low-Dimensional Carbon-Related Nanomaterials. Journal of Nanomaterials. 2011;2011:1-21.